Nexera UC Chiral CC4, 3um, 3.0 x 50mm LC/SFC Column

Nexera UC Chiral CC4, 3um, 3.0 x 50mm LC/SFC Column

Particle Size: 3 µm, Length: 50 mm

Part Number:

220-91626-01
Nexera UC Chiral CC4, 3 Micron, 3.0 x 50 mm The Nexera UC Chiral CC4 is a modified cellulose coated on high purity, high performance spherical silica particles. The chemical modification includes the chemical bonding of 4-chloro-3 methylphenylcarbamate to cellulose. The use of cellulose modified with chlorinated phenyl groups provides a separation opportunity for many previously unresolved and poorly resolved chiral mixtures. The Nexera UC Chiral CC4 columns are similar in selectivity to ChiralPak® OZ-H.

Part Number:

220-91626-01

Sign in to order

You are not allowed to see prices or add to cart. Please sign in, in order to start your order.

Sign in

Properties

ColumnID 3.0 mm
Length 50 mm
Particle Size 3 µm
By clicking 'Accept All' you consent that we may collect information about you for various purposes, including: Statistics and Marketing