Standard Ferrules
Phase Information: for 1/16-, 1/8-, and 1/4-Inch Fittings
Available in Vespel, graphite, or Vespel/graphite material.
Available in Vespel, graphite, or Vespel/graphite material.
Ferrule ID: 1/16"
Fitting Size: 1/16"
Material: VG2, 60% Vespel/40% Graphite
Product Name: Ferrules, Standard
Product Type: Ferrule
Similar to: Grace SF-100-VG2, 5132665