Shimadzu Part Number:REST-27488

SPME Arrow 1.10mm Polyacrylate thickness 100um, length 20mm, Color code grey

Restek PAL SPME Arrow • Rugged stainless steel construction ensures longer lifetimes. • Faster extraction means higher sample throughput. • Better sensitivity allows lower LODs. *These molecular weight ranges are a reasonable approximation; however, end users should verify suitability for their specific application. All Restek PAL SPME Arrows have 20 mm of phase bonded onto stainless steel. Color: Gray DF: 100 µm Diameter: 1.1 mm Material: Polyacrylate Product Name: SPME Arrow Product Type: Air Accessory Recommended Analytes: Polar, semivolatile, 80–300 g/mol* Units: ea.
Price: $476.00
×
In stock

These items are in stock and ready to ship.

Out of stock

These items are currently not in stock. Replenishment times may vary and can delay your order fulfillment. Please contact Customer Service for a recommended replacement if desired.

Special order

These items are not stored at a Shimadzu warehouse. They drop-ship to you directly from our suppliers and may delay your order fulfillment or arrive separately from other items in your order.

In stock