Dehydrator powder for high moisture content SFE samples. Includes 100 packets, 1g each. Use an equal amount of sample and dehydrator, then pack into the SFE extraction vessel. 5mL vessels require filter packing 228-59264-83 at the top and bottom of the vessel.