Stabilwax Columns
Material: (fused silica)
Phase Information: polar phase; Crossbond polyethylene glycol
• Rugged enough to withstand repeated water injections.
• Low-bleed PEG column ensures long column lifetimes.
• Temperature range: 40 °C to 260 °C.
• Equivalent to USP G14, G15, G16, G20, and G39 phases.
Restek’s polar-deactivated surface tightly binds the Carbowax polymer and increases thermal stability, relative to competitive columns. Because of the increased stability produced by the bonding process, Stabilwax columns exhibit long column lifetimes, even when programming repeatedly up to 260 °C. The bonding mechanism of the column also produces polar compound retention times that do not shift, as is often observed on other wax-type columns. In addition, this bonding mechanism produces a column that can be rejuvenated by solvent washing. Stabilwax columns are used for a wide range of compounds and matrices including: FAMEs, flavor compounds, essential oils, solvents, aromatics (including xylene isomers), acrolein/acrylonitrile (EPA 603), and oxygenated compounds. Also used for purity testing of chemicals and analyzing impurities in water matrices and alcoholic beverages.
Similar Phases: HP-INNOWax, CP-Wax 52 CB, VF-WAX MS, ZB-WAXplus
DF: 0.50 µm
ID: 0.25 mm
Length: 30 m
Product Name: Stabilwax
Product Type: GC Column
Similar to: Agilent 122-7333, 19091N-233
Similar to: Varian CP8746
Similar to: Grace 136472, 5121834
Temp Limits: 40 to 250/260 °C
Units: ea.