Rtx-5 Amine Columns
Material: (fused silica)
Phase Information: low-polarity phase; Crossbond 5% diphenyl/95% dimethyl polysiloxane
• Application-specific columns for amines and other basic compounds, including alkylamines, diamines, triamines, ethanolamines, and nitrogen-containing heterocyclics.
• Stable to 315 °C.
please note
We recommend using base-deactivated fused silica guard columns and base-deactivated liners with Rtx-5 Amine columns.
Active basic compounds that otherwise require derivatization, or an alternative analytical technique, can be analyzed on an Rtx-5 Amine column. The tubing surface is chemically altered to reduce tailing of basic compounds, eliminating the need for column priming. An Rtx-5 Amine column is ideal for analyzing a wide variety of basic compounds, but breakthrough technology also allows the analysis of neutral compounds, adsorptive compounds with oxygen groups susceptible to hydrogen bonding, or even weakly acidic compounds such as phenols. Every Rtx-5 Amine column is tested to ensure that it exceeds the requirements for analyzing ppm levels of amines, without priming, and to ensure low bleed at maximum operating temperature.
Similar Phases: Optima-5Amine
DF: 1.50 µm
ID: 0.32 mm
Length: 15 m
Product Name: Rtx-5 Amine
Product Type: GC Column
Temp Limits: -60 to 290/305 °C
Units: ea.