Rxi-1ms Columns
Material: (fused silica)
Phase Information: nonpolar phase; Crossbond dimethyl polysiloxane
• General-purpose columns for arson accelerants, essential oils, hydrocarbons, pesticides, PCB congeners (e.g., Aroclor mixes), sulfur compounds, amines, solvent impurities, simulated distillation, oxygenates, gasoline range organics (GRO), refinery gases.
• Tested and guaranteed for ultra-low bleed; improved signal-to-noise ratio for better sensitivity and mass spectral integrity.
• Temperature range: -60 °C to 330/350 °C.
• Equivalent to USP G1, G2, and G38 phases.
Rxi Capillary GC Columns
What do Rxi columns mean to you? Three things:
• Ultra-low bleed.
• Exceptional inertness.
• Reproducible performance, column after column.
Rxi fused silica capillary GC columns were designed specifically to be the best columns available, for exceptional inertness, ultra-low bleed, and reproducible retention and selectivity. In addition to outstanding performance, this combination of column characteristics assures Rxi columns will have long lifetimes. The Restek chemists also have developed a stable, reproducible manufacturing process, so that Rxi columns will meet your needs every time you install a new column.
Similar Phases: HP-1ms, HP-1msUI, DB-1ms, DB-1msUI, Ultra-1, VF-1ms, ZB-1, ZB-1ms
DF: 0.25 µm
ID: 0.25 mm
Length: 60 m
Product Name: Rxi-1ms
Product Type: GC Column
Similar to: Agilent 122-0162, 19091s-936
Similar to: Phenomenex 7KG-G011-11
Similar to: Grace 15941, 8635354
Temp Limits: -60 to 330/350 °C