Shimadzu Part Number: 339-89191-04

POLYETHYLENE SAMPLE, 10 G, CFT-EX

POLYETHYLENE SAMPLE, 10 G, CFT-EX. 10 g polyethylene sample for CFT-EX series capillary flow testers.
Price: $16.00