Nonporous cation exchange column for ultra-fast analysis. Polyhydroxymethacrylate base material with a sulfopropyl functional group. PEEK housing, shipping solvent is 20 mM MES (2-(N-Morpholino)ethanesulfonic acid) buffer (pH5.6). Ion exchange capacity: 0.2 meq/g.