The Mastro2 column has a biocompatible PEEK-lined stainless steel body with a high pressure polymer frit. This inertness eliminates adsorption and reduces tailing for compounds that tend to form chelates with metal surfaces, especially those containing phosphate groups. USP L1, 120A pore size, 340 m2/g surface area, 13% carbon load, endcapped. Maximum operating pressure is 40MPa/400 bar/6000 psi. pH: 2 - 7.5. Maximum temperature is 80C (pH 3 or higher.) Replacement for SSOT-G10001.