Column, GC, SH-MetalX-1HT SimDist, 5m x 0.53mm x 0.10um
Part Number:
227-36344-01
Stainless steel capillary simulated distillation column for accurate boiling point determination of medium and heavy fractions. Low bleed, 100% dimethyl polysiloxane phase suitable for ASTM D2887, D6352, D7169, D7213, and D7500. Coil diameter: 7", temperature range: -60 to 430/450C. Replacement for 220-94856-01 and 220-90604-03.
Part Number:
227-36344-01
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
Height | 2.50 in |
Length | 9.00 in |
Weight | 0.65 lbs |
Width | 9.00 in |