Shim-pack Velox Biphenyl, 5um, 4.6 x 250mm LC Column
Particle Size: 5 µm, Length: 250 mm
Part Number:
227-32018-04
The Shim-pack Velox Biphenyl offers complementary selectivity to alkyl phases (e.g. C8 or C18,) resulting in enhanced retention and resolution of aromatic compounds, especially with methanolic mobile phases. It is ideal for high-throughput LC-MS/MS bioanalytical applications such as drug and metabolite analysis. Recommended for large drug panels including barbiturates, benzodiazepines, opioids, stimulants, and more. The Velox superficially porous particle (SPP) provides UHPLC-like high speed, high resolution separations to reduce run time and increase sample throughput when run on a standard HPLC system. pH range 2-8, maximum temperature 80C, maximum pressure 400 bar/40 MPa/5800 psi.
Part Number:
227-32018-04
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
USP Designation | L11 |
Pore Size | 90 Ã… |
End Capping | Yes |
Carbon Load | 5% |
ColumnID | 4.6 mm |
Height | 1.80 in |
Length | 13.40 in |
Weight | 0.50 lbs |
Width | 2.80 in |
Length | 250 mm |
Max Temp | 80C |
Particle Size | 5 µm |
Phase | Biphenyl |