Properties
USP Designation | L1 |
Pore Size | 90 Ã… |
End Capping | Yes |
Carbon Load | 7% |
ColumnID | 2.1 mm |
Height | 1.00 in |
Length | 5.50 in |
Weight | 0.05 lbs |
Width | 1.50 in |
Length | 5 mm |
Particle Size | 2.7 µm |
Phase | C18 |