Ultra C18, 5um, 50 x 30mm Prep LC Column
Part Number:
REST-9174559
Ultra C18 is an endcapped, monomeric C18 (USP L1) suitable for the analysis of a wide range of compounds from acidic through slightly basic. Pore size: 100A, surface area: 300 m2/gram, carbon load: 20%, pH range: 2.5-8.0. Method development on an analytical Ultra C18 column is highly recommended before purchasing a prep column. Prep columns cannot be returned or exchanged once used.
Part Number:
REST-9174559
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
Height | 2.50 in |
Length | 9.00 in |
Weight | 0.30 lbs |
Width | 9.00 in |