Nexcol C18, 5um, 3.0 x 50mm LC Column
Particle Size: 5µm, Length: 50mm
Part Number:
220-91394-07
A traditional fully porous, endcapped C18 (USP L1) ideal for general-purpose use in reversed-phase chromatography. This is the installation checkout column included with new HPLC systems. Wide pH range (2–8) provides excellent data quality for many applications, matrices, and compounds. To add a guard column, use 220-91394-06 (3/pk) and holder 227-32041-01. For replacement ampules of test mix, use 220-91394-05. Pore size: 100A, surface area: 300m2/g, carbon load: 20%, pH range: 2-8, max temp: 80C, max pressure: 40 MPa/400 bar/5800 psi.
Part Number:
220-91394-07
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
USP Designation | L1 |
ColumnID | 3.0 mm |
Height | 1.80 in |
Length | 9.60 in |
Weight | 0.25 lbs |
Width | 3.40 in |
Length | 50mm |
Particle Size | 5µm |
Phase | C18 |