![Shim-pack Bio Diol-200, 2um, 4.6 x 30mm LC Column](/Admin/Public/GetImage.ashx?width=1280&image=%2fFiles%2fImages%2fProducts%2f227-31009-02.jpg&format=webp)
Shim-pack Bio Diol-200, 2um, 4.6 x 30mm LC Column
Part Number:
227-31009-02
Shim-pack Bio Diol: Size Exclusion Chromatography Columns. With different pore sizes, Shim-pack Bio Diol LC columns are effective for analysis of aggregates and fragments of mAb, oligonucleotides and carbohydrates. Diol-200
Particle:Silica
Ligand: Dihydroxypropyl (Diol)
Particle Size: 2?m, 3?m, 5?m
Pore Size: 6 nm 12 nm 20 nm 30 nm
pH Range: 5.0 – 7.5
Molecular Weight Range: 5,000 – 300,000