![Shodex GPC KF-805L, 10um, 8.0 x 300mm LC Column](/Admin/Public/GetImage.ashx?width=1280&image=%2fFiles%2fImages%2fProducts%2f220-91524-40.jpg&format=webp)
Shodex GPC KF-805L, 10um, 8.0 x 300mm LC Column
Particle Size: 10 µm, Length: 300 mm
Part Number:
220-91524-40
Styrene divinylbenzene copolymer-based mixed-gel column capable of analyzing samples over a wide range of molecular weights. Target molecular weight range = 300 - 2,000,000. Exclusion limit = 4,000,000. Fulfills USP L21 requirements. Shipping solvent is THF and can be converted to chloroform, DMF, and several other solvents for multiple applications. Contact Shimadzu technical support for the complete list. Replacement for K-805L, 220-91524-16 which is shipped in chloroform. Contact Shimadzu for the solvent exchange procedure to use KF-805L with chloroform.
Part Number:
220-91524-40
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
ColumnID | 8.0 mm |
Height | 2.20 in |
Length | 15.80 in |
Weight | 0.90 lbs |
Width | 3.40 in |
Length | 300 mm |
Particle Size | 10 µm |