Capillary Tubing, SS 1/16"OD x 0.007 ID x 10cm L, 3-pk Yellow
Part Number:
REST-25818
LC Stainless Steel Capillary Tubing
• 316-grade stainless steel.
• Precise precut lengths.
• Clean and smooth surface finish.
• Color coded for easy identification.
• Tight tolerance: OD and ID +/-0.001".
Whether you need to replace system tubing as part of your troubleshooting or want to reduce the dwell volume of your system as you move to narrower columns, Restek has the quality tubing in the lengths and IDs you need. Each ID is color coded, so it is easy to identify and replace correctly. Tubing is precision cut, resulting in clean, square-cut ends without ovality.
Color: yellow
ID: 0.007" (0.178 mm)
Length: 10 cm
Material: 316-grade stainless steel
Max Pressure: 26,610 psi
OD: 1/16"
Product Name: LC Capillary Tubing
Product Type: HPLC Accessory
Similar to: 25245 (discontinued)
Units: 3-pk.
Part Number:
REST-25818
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
Height | 0.50 in |
Length | 4.20 in |
Weight | 0.10 lbs |
Width | 0.10 in |