EXP Ferrule Titanium Hybrid, ea
Part Number:
REST-25935
Reusable titanium/PEEK hybrid ferrule for UHPLC connections. Hand-tight with the original EXP fitting to 8,700 psi, or up to 20,000 psi with the EXP2 nut and driver. For 1/16" OD stainless steel tubing. Not recommended for PEEK tubing. Use with any EXP or EXP2 fitting. Replacement for 220-91522-33.
Part Number:
REST-25935
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
Height | 0.50 in |
Length | 5.00 in |
Weight | 0.10 lbs |
Width | 3.00 in |