![EXP Hand-Tight Fitting w/Hybrid Ferrule, 10/pk](/Admin/Public/GetImage.ashx?width=1280&image=%2fFiles%2fImages%2fProducts%2f220-91522-36.jpg&format=webp)
EXP Hand-Tight Fitting w/Hybrid Ferrule, 10/pk
Part Number:
220-91522-36
Knurled fitting for UHPLC connections. Must be used with EXP titanium/PEEK hybrid ferrules. The ferrule is not permanently swaged to the tubing so it is reusable multiple times. Hand-tight to 8,700 psi and wrench-tight (7/16") to 20,000 psi. When using a wrench, for best results, tighten a maximum of 1/4 to 1/2 turn past hand tight. For 1/16" OD stainless steel tubing. Replacement ferrules are 220-91522-33 (ea) or 220-91522-34 (10/pk). Not recommended for PEEK tubing.
Part Number:
220-91522-36
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
Height | 0.20 in |
Length | 4.40 in |
Weight | 0.10 lbs |
Width | 2.80 in |