![Nexera 1-Piece SUS Fingertight Fitting. Not for 15/18 Valves](/Admin/Public/GetImage.ashx?width=1280&image=%2fFiles%2fImages%2fProducts%2f220-91522-04.jpg&format=webp)
Nexera 1-Piece SUS Fingertight Fitting. Not for 15/18 Valves
Part Number:
220-91522-04
One-piece reusable high pressure fitting. Stainless steel with polymer front cone, for pressures up to 11,000 psi. Fittings have a polymer wing at the top so it can be hand-tightened. Use for LC-30AD or LC-40 connection to mixer, SIL-30 and SIL-40 connection to mixer and columns, and CTO-30 connection to column(s). For 15K and 18K psi valves, use the longer stem fitting 220-91522-03.
Part Number:
220-91522-04
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
Height | 5.60 in |
Length | 5.60 in |
Weight | 0.20 lbs |
Width | 0.04 in |