Nexera UC Chiral CCJ, 3um, 4.6 x 150mm LC/SFC Column
Particle Size: 3 µm, Length: 150 mm
Part Number:
220-91625-35
Nexera UC Chiral CCJ, 3 Micron, 4.6 x 150 mm The Nexera UC Chiral CCJ (cellulose 4-methylbenzoate) is a robust column for high resolution chiral separations based on a halogenated carbohydrate based chiral stationary phase. Similar in selectivity to ChiralPak® OJ-H.
Part Number:
220-91625-35
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
USP Designation | L80, L107 |
ColumnID | 4.6 mm |
Length | 150 mm |
Particle Size | 3 µm |