Short Path Cuvette, Quartz, 1 mm PL, 350 µL, UV
Length: 1 mm
Part Number:
220-92910-41
Material: QS (Quartz), Light Path:1mm, Outside Dim.: 45x12.5mm, Inside Width:9.5mm, Base Thickness:1.5mm, Vol.:350µL, Window:2, Includes: PTFE lid. Requires spacer - 204-21473-03.
Part Number:
220-92910-41
Sign in to order
You are not allowed to see prices or add to cart. Please sign in, in order to start your order.
Properties
Height | 1.50 in |
Length | 3.00 in |
Weight | 0.05 lbs |
Width | 2.25 in |
Length | 1 mm |
Material | Quartz |
Volume | 350µL |